| Name |
Viscosity |
Solid(%) |
Solvents |
Modulus(Mpa) |
Tensile Strength(Mpa) |
Elongation(%) |
Number |
Characterstics |
Applicatons |
| Gloss resin | 500~1500 | 39.0~41.0 | DMF/MEK | | | | DRR-2911 | Yellowing style,gloss effect | PU surface treating |
| High soild gloss resin | 2000~3000 | 48.0~52.0 | DMF/TOL | | | | DRR-2910 | Yellowing style,high soild gloss effect,good brightness,strong crystal effect,water tumbling,strong stereoscopic effect | PU surface treating |
| High soild gloss resin | 5000~10000 | 48.0~52.0 | DMF/MEK | | | | DRR-2998 | Yellowing style,high soild gloss effect,good brightness,strong crystal effect | PU surface treating |
| High soild mirror resin | 9000~13000 | 29.0~31.0 | DMF/MEK | | | | DRR-2918 | Mid-hard type,good mirror effect | Suit for enamel-type leather |
| Crackle gloss resin | 1000~1200 | 37.0~39.0 | DMF/BAC/ACET | | | | DRR-2978 | Gloss and crackle effort ,smooth,good transparency,anti-abrasion | PU post treatment |
| Crackle resin(soft) | 1000~1200 | 37.0~39.0 | DMF/BAC/ACET | | | | DRR-2739 | Natural brightness,soft crackle effect,strong adhesion,strong real leather effort,smooth and natural hand touch feeling | PU post treatment |
| Pour suitable hair yangbuck burnish resin | 2500~3500 | 19.0~21.0 | TOL/MEK | | | | DRR-2555 | Pour suitable hair effort,darker after burnish,good hand touch feeling | Synthetic leather post treatment |
| Pour suitable hair yangbuck resin | 2500~3500 | 17.0~19.0 | MEK/TOL | | | | DRR-2587 | Strong hair effect,good hand touch feeling | Synthetic leather post treatment |
| Rough yangbuck resin | 800~1200 | 16.0~18.0 | IPA/TOL | | | | DRR-2527 | Strong fuzz waxy effect | PU post treatment |
| Thin yangbuck resin | 800~1200 | 16.0~18.0 | IPA/TOL | | | | DRR-2526 | Strong fuzz waxy effect | PU post treatment |